How to inspect the installation of plastic wood flooring?

2023/4/6

With the widespread use of plastic wood flooring, everyone should master the engineering acceptance method after the installation of plastic wood flooring. Is the color tone of the plastic wood flooring consistent? If the color deviation is large, it immediately harms the aesthetics and elegance, and can be replaced according to regulations; If the tone is too consistent and there is basically no color deviation, it depends on whether the patterns on the surface of the wooden floor are the same. If the patterns are similar, then it is possible that the processed plastic wood flooring is the material, rather than the precious wood flooring. Nowadays, some wood flooring raw material dealers choose ordinary wood materials, but apply a layer of precious wood types on the surface to fake and inferior wood flooring. The back is pasted with aluminum foil, which is said to be used for waterproofing. In fact, they are afraid of being seen with different patterns on the back and the reverse.


Are there holes, gaps, and scratches on the surface of plastic wood flooring? It is common because the ground keel has not been resolved and there are wood borers inside. By the time it was discovered that there was eye decay, the wooden floor had already been almost eaten away; Gaps and scratches can be understood at a glance. Standard requirement: The gap between wooden floors should not exceed 0.5mm; Scratches are mainly caused by the unsmooth interior decoration, and if they cannot be repaired by waxing, they must be replaced. Is there a sound in the plastic wood floor? When walking back and forth on the wooden floor during engineering acceptance, the pace must be intensified. Pay more attention to the position of the wall and door leaf during engineering acceptance. If there is a sound, walk repeatedly, clarify the specific address of the sound, and mark it properly. When encountering such situations, it is possible to stipulate dismantling and repaving. The location with noise is caused by the construction team's non-standard operation and inadequate application of raw materials throughout the entire construction process. The key to non-standard actual operation is reflected in the fixed and unstable ground keel; The key issue with poor raw materials is that the ground keel has not been air dried. Some decoration engineering companies use non dried ground keel construction, and when dry marks are seen on the surface, they actually do not dry.


The moisture content of plastic wood raw material products should be controlled at around 12% for ground keels with high moisture content. During the drying process of wood, the volume will decrease, leading to loosening. Once again, the engineering acceptance is to check whether the wooden floor is deformed or shrunk. The method of engineering acceptance is to use a two meter long scale, lean against the wooden floor, and the flatness should not exceed 3mm.